叶勇军,周乐,李梦艺,夏铭,刘淑媛.瓷砖地板接缝与非接缝处氡析出差异的实验研究[J].南华大学学报(自然科学版),2022,(3):1~7.[YE Yongjun,ZHOU Le,LI Mengyi,XIA Ming,LIU Shuyuan.Experimental Study on the Difference of Radon Exhalation Between Joint and Non-joint of Ceramic Tile Floor[J].Journal of University of South China(Science and Technology),2022,(3):1~7.]
瓷砖地板接缝与非接缝处氡析出差异的实验研究
Experimental Study on the Difference of Radon Exhalation Between Joint and Non-joint of Ceramic Tile Floor
投稿时间:2021-12-02  
DOI:
中文关键词:    楼板  氡析出率  局部静态法  氡眼
英文关键词:radon  floor  radon exhalation rate  local static method  Radon Eye
基金项目:国家自然科学基金项目(11575080)
作者单位E-mail
叶勇军 南华大学 资源环境与安全工程学院,湖南 衡阳 421001 yongjunye@163.com 
周乐 南华大学 资源环境与安全工程学院,湖南 衡阳 421001  
李梦艺 南华大学 资源环境与安全工程学院,湖南 衡阳 421001  
夏铭 南华大学 资源环境与安全工程学院,湖南 衡阳 421001  
刘淑媛 南华大学 资源环境与安全工程学院,湖南 衡阳 421001  
摘要点击次数: 397
全文下载次数: 205
中文摘要:
      为了探究缝隙的存在对建筑结构表面氡析出的影响,采用局部静态法,以机房、客厅、实验室贴瓷砖的地面为对象,测量了瓷砖与瓷砖接缝处的一字缝和十字缝以及非接缝处即瓷砖表面的氡析出率。结果表明:1)接缝处的集氡罩内平衡氡浓度远高于瓷砖表面;2)不同瓷砖表面的氡析出率不同,客厅、机房、实验室分别是0.327 mBq/(m2·s)、0.413 mBq/(m2·s)、0.072 mBq/(m2·s);3)一字缝、十字缝及瓷砖表面的氡析出率相差很大,在机房、客厅、实验室三处地面,一字缝表面氡析出率分别是瓷砖表面的3.19倍,2.43倍,2.25倍,十字缝表面的氡析出率分别是瓷砖表面的7.95倍、11.36倍、6.25倍。
英文摘要:
      To explore the influence of the existence of gaps on radon exhalation on the surface of building structures, the radon exhalation rate of single and cross joints and non-joints of ceramic tile surface was measured by using local static method on the ground covered with ceramic tile in computer room, living room and laboratory. The results show that:(1) The equilibrium concentration of radon in the radon collecting enclosure at the joint is much higher than that on the ceramic tile surface; (2) The radon exhalation rate of different ceramic tile surface is different, which is 0.327 mBq/(m2·s) in living room, 0.413 mBq/(m2·s) in computer room and 0.072 mBq/(m2·s) in laboratory; (3) The radon exhalation rate on single joints, cross joints and ceramic tile surface has huge difference. In the computer room, living room and laboratory, the radon exhalation rate on single slit surface is 3.19 times, 2.43 times, 2.25 times of that on ceramic tile surface respectively. The radon exhalation rate on cross slit surface is 7.95 times, 11.36 times, 6.25 times of that on ceramic tile surface respectively.