邱亮,赵玉宝,樊造,刘彪,欧阳兵.BiOBr可见光催化降解环丙沙星的晶面依赖性能[J].南华大学学报(自然科学版),2016,30(2):103~106.[QIU Liang,ZHAO Yu-bao,FAN Zao,LIU Biao,OUYANG bing.Facets-dependent Performance of BiOBr for PhotocatalyticDegradation of Ciprofloxacin Under Visible Light[J].Journal of University of South China(Science and Technology),2016,30(2):103~106.] |
BiOBr可见光催化降解环丙沙星的晶面依赖性能 |
Facets-dependent Performance of BiOBr for PhotocatalyticDegradation of Ciprofloxacin Under Visible Light |
投稿时间:2016-03-08 |
DOI: |
中文关键词: 晶面 光催化 环丙沙星 速率常数 |
英文关键词:facet photocatalysis ciprofloxacin rate constants |
基金项目:湖南省教育厅科学研究优秀青年基金资助项目(13B100) |
|
摘要点击次数: 779 |
全文下载次数: 920 |
中文摘要: |
采用水热法制得了分别择优暴露{110}、{010}和{001}晶面的BiOBr.XRD研究结果显示,相应样品{110}与{102}衍射峰的强度之依次减小;可见光下BiOBr光催化降解环丙沙星的实验结果表明,BiOBr{110}、BiOBr{010}和BiOBr{001}上环丙沙星降解反应速率常数依次为0.008 9、0.001 2和0.000 9 min-1,即暴露的{110}晶面越多,其光催化降解环丙沙星的活性越高.BiOBr {110}晶面具有强的内电场,应是其高催化性能的内在原因. |
英文摘要: |
The BiOBr samples with {110},{010} or {001} facets were obtained by hydrothermal methods.The results of XRD show that their intensity ratios of diffraction peak {110} to {102} decrease accordingly.The reaction rate constants of BiOBr{110},BiOBr{010} and BiOBr{001} for photocatalytic decomposing ciprofloxacin under visible light irradiation were 0.008 9,0.001 2 and 0.000 9 min-1,respectively.That is to say,the more the {110} facets exposed,the higher the photocatalytic efficiency of BiOBr.The strong internal electric field of BiOBr with {110} facets is shown to be the intrinsic factor for its high photocatalytic performance. |